Two-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: comp. A : comp. B = 3 : 1. Pot life of mix:…
Two-component, anti-corrosion cementitious mortar for steel reinforcement rods.…
One-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: 100 parts of MAPEFER 1K with 20-22 parts of…
One-component, anti-corrosion cementitious mortar for steel reinforcement rods.…
MAPEFER 1K ZERO is a one-component mortar made from cementitious binders, powdered polymers and corrosion inhibitors and is applied to steel reinforcement to prevent the formation of rust and as an…
MAPEFER 1K ZERO is a one-component mortar made from cementitious binders,…
Two-component cementitious mortar with a low modulus of elasticity for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT BM comp. A with…
Two-component cementitious mortar with a low modulus of elasticity for…
Fibre-reinforced, quick setting and hardening, compensated-shrinkage mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 1 mm. Mixing ratio: 100 parts of MAPEGROUT FAST-SET…
Fibre-reinforced, quick setting and hardening, compensated-shrinkage mortar for…
Medium-strength (40 MPa), compensated-shrinkage fibre-reinforced thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT T60 with 16.5-17.5 parts…
Fibre-reinforced, sulphate-resistant thixotropic mortar for repairing concrete.…
Fibre-reinforced, compensated-shrinkage mortar for repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT TISSOTROPICO with 15.5-16.5 parts…
Fibre-reinforced, compensated-shrinkage mortar for repairing concrete.…
Fibre-reinforced, compensated-shrinkage mortar for
repairing concrete. TECHNICAL DATA: Maximum dimension of aggregate: 2.5 mm. Mixing ratio: 100 parts of MAPEGROUT THIXOTROPIC E with 15.5-16.5 parts…
Fibre-reinforced, compensated-shrinkage mortar for
repairing concrete.…