Pultruded carbon fibre plate impregnated with epoxy resin with a protective plastic film on both faces. TECHNICAL DATA: Modulus of elasticity: 170 - 200 - 250 GPa. Fibre content: 68% - 68% - 65%.…
Pultruded carbon fibre plate impregnated with epoxy resin with a protective…
Pultruded carbon fibre tube impregnated with epoxy resin for reinforced injections in masonry. TECHNICAL DATA: Tensile modulus of elasticity: 170,000 N/mm ² . Content of fibre by weight: 68%. Tensile…
Pultruded carbon fibre tube impregnated with epoxy resin for reinforced…
Reversible consolidator in solvent for the conservative restoration of porous stone substrates, lime render and layers of paint. TECHNICAL DATA: Dry solids content: 3%. Storage: 12 months.…
Reversible consolidator in solvent for the conservative restoration of porous…
Elastomeric, crack-bridging, permanently flexible, protective paint with high resistance to chemicals for internal and external surfaces. TECHNICAL DATA: Consistency: thick liquid. Colour: white or…
Elastomeric, crack-bridging, permanently flexible, protective paint with high…
Solvent-based high-penetration consolidating primer to even out surfaces. TECHNICAL DATA: Consistency: fluid liquid. Colour: transparent. Density (EN ISO 2811-1) (g/cm ³ ): approx. 0.96. Dry solids…
Solvent-based high-penetration consolidating primer to even out surfaces.…
Two-component, super-fluid epoxy resin applied by injecting. TECHNICAL DATA: Mixing ratio: comp. A : comp. B = 4 : 1. Pot life of mix: 40 minutes (at +23°C). Classification: EN 1504-5 and EN 1504-6.…
Two-component, super-fluid epoxy resin applied by injecting. TECHNICAL DATA:…
Two-component epoxy resin with a very low viscosity for injecting into micro-cracks. TECHNICAL DATA: Mixing ratio: comp. A : comp. B = 4 : 1. Pot life of mix: 70 minutes (at +23°C). Classification:…
Two-component epoxy resin with a very low viscosity for injecting into…
Two-component, anti-corrosion cementitious mortar for steel reinforcement rods. TECHNICAL DATA: Maximum dimension of aggregate: 0.5 mm. Mixing ratio: comp. A : comp. B = 3 : 1. Pot life of mix:…
Two-component, anti-corrosion cementitious mortar for steel reinforcement rods.…