LIVIGUM

Syntetic-resin based admixture in water dispersion to be added to cementitious mortar and smoothing compounds to improve mechanical performances and adhesions.
Mixing ratio:
1. Preparation of skim layers and render up to 10 mm thick. Dilute LIVIGUM with water at a ratio of 1:2. Use this solution to mix the aggregates and cement.
2. Preparation of skim layers and render up to 20 mm thick. Dilute LIVIGUM with water at a ratio of 1:3. Use this solution to mix the aggregates and cement.
3. Admixture for PIANOCEM M. Partially replace the mixing water with 1.5-2 kg of LIVIGUM every 25 kg bag.
4. Primer for cementitious substrates. Dilute 1 part of LIVIGUM with 3-5 parts of water, according to the absorption of the substrate.
Consumption: 60-90 g/m² per mm of skimming; 1,5-2 kg bag of PIANOCEM M.
Packaging: 25 kg tanks.

Related documentation

Technical data sheet
Download
Safety Data Sheet
Download

Last Projects LIVIGUM

Category icon PUBLIC BUILDINGS AND URBAN DESIGN

2016/2018

Lega del Filo d’Oro National Centre

Osimo, Italy

Facades maintenance

Category icon COMMERCIAL FACILITIES

2016/2017

CityLife Shopping District

Milan, Italy

Installation of floors

Category icon COMMERCIAL FACILITIES

2016

RELAIS CHATEAU DE MIRAMBEAU

MIRAMBEAU, France

Installation of floors

Category icon INFRASTRUCTURES

2014

Stazione Ferroviaria Termini

roma, Italy

Installation of floors

Keep in touch

Subscribe to our newsletter to get Mapei news