Create a smoothing layer with one-component cementitious-base ready mixed thixotropic mortar, so that a smooth coat for the subsequent application of finishing layers is obtained.
Create the protection layer by applying three-component epoxy-cementitious thixotropic mortar by spray through screw pump and subsequent spreading using a metal trowel.